EN 1.4435
Stainless austenitic acid resistant steel – Stock standard
Product standard:
EN 10088-3
EN 10272
Material standard:
W.Nr.1.4435
EN 1.4435
DIN X2CrNiMo18-14-3
(~AISI 316L) 
Material description:
EN 1.4404 is a stainless austenitic chrome-nickel-molybdenum steel. The increased content of Chromium, Nickel and Molybdenum improves the corrosion resistance in comparison to EN 1.4404 steel.
Chemical analysis (%):
| Element: | EN 1.4435 | 
| Carbon [C] max. | 0,03 | 
| Silicon [Si] max. | 1,00 | 
| Manganese [Mn] max. | 2,00 | 
| Phosphorus [P] max. | 0,045 | 
| Sulphur [S] max. | 0,015 | 
| Chromium [Cr] | 17,0 – 19,0 | 
| Molybdenum [Mo] | 2,50 – 3,00 | 
| Nickel [Ni] | 12,50 – 15,00 | 
| Nitrogen [N] max. | 0,11 | 
| Iron [Fe] | Rest | 
Mechanical properties:
Tensile strength, Rm: 600 – 950 MPa. (deviations possible) 
Condition:
2H: Solution annealed (+AT), cold drawn (+C)
Technical properties:
Straightness: ≤ 1,00 mm / 1000 mm 
Delivery form:
Lengths of 3000 mm (±50 mm)
Tolerances:
According to DIN EN 10278 – ISO h09
| Diameter: | ISO h08 [mm] | ISO h09 [mm] | 
| >1 till 3 | +0/-0,014 | +0/-0,025 | 
| >3 till 6 | +0/-0,018 | +0/-0,030 | 
| >6 till 10 | +0/-0,022 | +0/-0,036 | 
| >10 till 18 | +0/-0,027 | +0/-0,043 | 
Stock dimensions:
| Dia. [mm] | Tol. EN ISO | Rm [MPa] | Ends | 
| 15,0 | h9 | 600 - 950 | Chamfered | 
Other dimensions are offered on request.
Typical applications:
Machined parts for use in corrosive environments. 
Tests and certificates:
Certificate according to EN 10204/3.1. 
The products comply with the requirements of:
- EN 10272/08
- AD2000 Merkblatt W0/W2 and PED 2014/68/EU
Intergranular Corrosion Test according to ASTM A262/15 E Method - EN ISO 3651-2/1998